Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CP PRYME® ABS A100HI-85 - ABS - Chase Plastics

Material Data Center offers the following functions for CP PRYME® ABS A100HI-85:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other CP Pryme datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 15 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
ASTM Data
Indice de fluidité, MFI 3.7 g/10min ASTM D 1238
Température 230 °C -
Charge 3.8 kg -
Retrait au moulage , parallèle 0.0065 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module en traction 2070 MPa ASTM D 638
Module de traction d’élasticité 41.4 MPa ASTM D 638
Résistance de traction à la rupture 31.7 MPa ASTM D 638
Allongement d’élasticité 2.1 % ASTM D 638
Allongement à la rupture 26 % ASTM D 638
Module de flexion 2140 MPa ASTM D 790
Résistance à la flexion 68.3 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 370 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 97.2 °C ASTM D 648
DTUL à 264 psi 82.2 °C ASTM D 648
Vicat température 98.9 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Densité 1050 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 82 - 93 °C -
Pré-séchage - temps 2 - 4 h -
L'humidité de traitement ≤0.1 % -
Température du moule 49 - 71 °C -
Zone 1 188 - 210 °C -
Zone 2 204 - 227 °C -
Zone 3 216 - 238 °C -
Température de la buse 218 - 260 °C -
Contre-pression 0.345 - 0.689 MPa -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Propriétés spéciales
Modifié choc
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.